[Table of Contents] [Search]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

non-ionic surfactants



Assuming room temperature, what is the critical micelle concentration of the
non-ionic surfactant Synperonic N?  Timar-Balazsy and Eastop give a range
for non-ionics of .05g/L to 0.5g/L; an internet search has not yielded much
specific info.  I am curious what concentration people are using. Thanks,
Anne Peranteau
Mellon Fellow in Textile Conservation
Philadelphia Museum of Art


[Subject index] [Index for current month] [Table of Contents] [Search]