[Table of Contents] [Search]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

Re: 108" wide bleached and unbleached double napped cotton flannel



Please note that Testfabrics, Inc. now has 108" wide, double napped (front
and back) cotton flannel in both unbleached (style 425U XW) and bleached
(style #425 XW). Prices, samples etc. available on request to Tom Klaas,
email address: testfabric@xxxxxxx