Another source for terms is the ASTM (American Society for Testing and Materials) D 3990-93 (reapproved 1998) Standard Terminology Relating to Fabric Defects.
Crocking is defined as a color transfer from one fabric surface to another by rubbing. Foxing and foxy are not mentioned.
More information on ASTM and standards can be found at http://www.astm.org