I need help from the collective again. We have received 80,000
unique KS aerial black & white photos dating from 1950's-1970
from the US Dept. of Agriculture. Due to improper storage over
the years, many are badly curled. We have tried putting a small
amount in a book press for several weeks with no success. Is
there anything else we can do or do you have any suggestions to
where they can be worked on? (We do not have a conservator on
staff.) I'm thinking about posting it to CONS Dist List.