Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Removing silking

Removing silking

From: Barry Knight <drbarryknight<-at->
Date: Tuesday, October 6, 2015
Ala Rekrut <ala.rekrut<-at->gov<.>mb<.>ca> writes

>...   I would
>appreciate any treatment suggestions, recommendations of currently
>available alpha amylase enzymes, or observations on silking that
>might lead to alternate treatment directions.

Just a thought, but instead of using amylase to dissolve the
adhesive, have you considered using a proteolytic enzyme to dissolve
the silk--or at least, the recalcitrant parts that cannot be removed
with hot water?

Barry Knight
St Albans
England


                                  ***