Subject: Anoxia and plastics

Anoxia and plastics

From: Mary-Lou Florian <mflorian<-a>
Date: Monday, June 20, 2011
Ingrid Neuman <berkart [at] earthlink__net> writes

>I am curious if anyone has thought about, is looking into or
>currently experimenting with anoxic encapsulation of small
>contemporary art pieces composed of plastics (in Escal for instance
>with Ageless) in order to slow down the rate of deterioration of
>certain types of polymers? ...

You might look into oxygen adsorber sachets that are used
commercially.  They're inexpensive but have a life time.

Mary-Lou Florian


                                  ***