Marcin Kozarzewski <koza [at] pagi__pl> writes

>Keim colours and other silicate colours for murals
>
>I am searching for various information about the mineral, silicate
>colours for the murals like Keim Colours and its modifications. I
>search for the following items:

In march 1997 a conference on silicate paint took place at the ETH
Zurich, Switzerland, which was published as a book in 1998:
Mineralfarben: Beitrage zur Geschichte und Restaurierung von
Fassadenmalereien und Anstrichen. Weiterbildungstagung, 20.-22. Marz
1997. 1998, vdf, Hochschulverlag, ETH Zurich.

Diverse authors write about the history, use, chemical and technical
problems of the use of Keim paint. All papers are published in
German.

Dr. Christine Blaeuer Boehm
BCD GmbH
Wankdorffeldstr. 102, PF 261, CH-3000 Bern 22
+41 31 335 62 12 or
+41 81 252 59 84
Fax: +41 81 253 69 48


                                  ***
                  Conservation DistList Instance 13:47
                  Distributed: Tuesday, March 14, 2000
                       Message Id: cdl-13-47-005
                                  ***
Received on Friday, 10 March, 2000

[Search all CoOL documents]


Feedback for CoOL webmaster