Ginny Rosner <grosner [at] indianahistory__org> writes

>If no one knows the whereabouts of Atlantic Protective Pouches, can
>you tell us of any other supplier of mylar that would make folders
>and L-sleeves to our size specifications, and does not require a
>minimum order?

The best two suppliers of this product I know of in terms of cost
and quality would be worth contacting--usually they will work with
you on small quantities, but do keep in mind if its very small the
per sleeve cost might be fairly high.

    KR Plastics (in Austin, TX)
    512-462-2821

or

    University Products (Holyoke, MA)
    800-628-1912