Yangsook Choe <ysc [at] foremalsvard__bd__se> writes

>I would like to hear your experiences and to discuss, for
>example, about a best temperature for the best results and how you
>applying it and why?, etc. I am also interested in any tips for
>books and articles about this subject.

Try to contact:

    Mr. Lemaire, Laboratoire d'Archeologie des Metaux
    Musee de l'histoire du Fer
    Av. du General de Gaulle - BP 15
    54140 Jarville - La Malgrange
    France
    <URL:http://www.ot-nancy.fr/patrimoine/musee/m_fer.htm>

                                  ***