This query is posted on behalf of a colleague in Greece: Please
reply to this if you have any useful knowledge. It is urgent.

    1.  Is it really possible, using Art-Sorb, to maintain RH levels
        as low as 2% in display cases?

    2.  Is it impossible to achieve this with silica gel?

    3.  If the results between the two methods are close, is it
        worth paying the extra money for Art-Sorb: ie. does it last
        longer, or is more reliable.

    4.  If these questions have already been addressed in any
        publication, please let us know where.

Nigel Larkin,
Norfolk Museums Service, and Palaeontological & Archaeological
    Services Ltd.
Chateau De La Lune
3 Park Lane
Scarning, Dereham, Norfolk NR192LD
+44 1362 860915
Fax:+44 1362 860385)
+44 1362 687760 (home)
+44 973 869613 (mobile)

                                  ***
                  Conservation DistList Instance 11:32
                  Distributed: Monday, October 6, 1997
                       Message Id: cdl-11-32-003
                                  ***
Received on Wednesday, 1 October, 1997

[Search all CoOL documents]


Feedback for CoOL webmaster