Scott Campbell <ScottCampbell<-a t->adidam< . >org> writes

>Is anyone aware of a ballpoint pen or rollerball pen that uses
>permanent black ink? The pen must be capable of surviving in a
>tropical environment as well as being able to work in an
>air-conditioned space without skipping, smearing, bleeding through,
>fading, etc.

Scott Campbell does not say what he is going to write on with the
pens. If it is paper or fabric, Pigma Pens would work. They come
in many widths and are fade proof and water proof.

Cathy Atwood
Local Records Program, Missouri Secretary of State

                                  ***