The stencil burner model SB 1, 120V 20W 60HZ, 513F from UL, Air
Nouveau 908-364-2111, Lakewood, NJ 08791 makes a very good heated
microspatula. To control the temperature one can use a light dimmer,
which is also an inexpensive device.

                                  ***