At the Media Laboratory at the National Library of Norway we
microfilm on, copy  and process Cibachrome film stock. For some
reason Ilford is playing this game with their cards close to their
chest, that is to say, they don't give out much information on
chemistry and QC of it. Are there anyone out their with similar
problems or experience with Cibachrome who would like to join a
e-mail discussion group on this subject, please take contact with me
and will set up a group operation here at the library.