We have done a study on several varieties of foil backed labels with the
same results, they don't work. After a short period of time they begin
to lift. The labels were tested on paper backed books which has a
similar texture to microfilm boxes. We put the labels on, sent the
books to the shelf, then retrieved them after two weeks. In almost every
case the label was no longer flat.

                                  ***