Sue:
Check with the Library Binding Service (LBS) which used to shrink wrap
returned brittle volumes with multiple loose pages.

Erich J. Kesse
Preservation Office
University of Florida Libraries
904-392-6962
Fax: 904-392-7251

                                  ***