A while back I notified this list that tape backing
of polyester tape was beginning to fail.

This, as it develops, was incorrect.  It was
environmenal chamber that was gradually failing, finally ceasing to work at all-
the little light which showed the temperature system was
working didn't come on any more.

When the control card was replaced, it operated
correctly and baking results were as before- successful.