Robert

Shamrock was the name Ampex used instead of selling junk tape in
white boxes.

After tape is made and before it is packaged, a certain percentage
of the batch/run would be tested--something like four from select
parts of a single sheet (web) of basefilm.  If these tapes did not
pass the test, every tape in that web was "white-boxed" and sold to
K-Mart-type stores.  The name Ampex does not appear anywhere on the
reel or the box.  Let the Buyer Beware!

Of course, four tapes doesn't mean the other 1,000 tapes are
bad--some could be great.  I will never forget a Consumer Reports
article comparing reel-to-reel audio tapes and Shamrock was the best
in the world! The State of California bought millions of reels of
Shamrock from the lowest bider.

Jim Wheeler