Re: [ARSCLIST] Pre-echoes/ post echoes



David Breneman wrote:
--- On Sun, 8/17/08, Ward Duffield <wardd@xxxxxxxxxxx> wrote:


buy
t no real closure on this.
Opinions, anyone?

It's caused by magnetic print-through from one wrap of the master tape resting against another on the reel on which it was stored.

>

Also from over-cutting.