At 12:11 PM 10/29/2007, you wrote:
IASA recognises this as an acceptable cleaning method. The IASA document 'Guidelines on the production and preservation of digital audio objects' (TC-04) states;

'An ultrasound bath using a liquid that is not a solvent for the recording surface will increase throughput. The depth need not be more than the radius of a disc recording and the recording is suspended on a shaft parallel to the liquid surface and such that the label area is not submerged. The effect of all solvents should be tested before use' (Paragraph 5.2.3.4)

'As with historical mechanical and other obsolete formats ... ultrasonic cleaning may be effective. Care should be taken in the selection of solvent, though a 1% solution of Cetrimide in distilled water is an appropriate cleaning solution. The label should be kept clear of the fluid, and the disc rotated slowly until the whole grooved area has been wetted.' (Paragraph 5.3.3.4) [Note: this paragraph is referring specifically to vinyl discs]

The British Library Sound Archive use an ultrasonic bath for vinyl and for shellac records that are particularly dirty with grit or soot etc before washing on a Keith Monks machine. The record is 'dipped' with a rod passing through the spindle hole so that the label is clear of the bath and is slowly turned by hand whilst the bath is operating so that the surfaces are cleaned. The liquid in the bath is distilled water and a record is cleaned for typically 20 seconds. We don't use the ultrasonic bath on cracked or damaged records but we consider both vinyl and shellac to be resilient and not to suffer from the process.

Thanks for the explanation. I can see how ultrasonic cleaning would be suitable for vinyl, as you are dealing with an impermeable surface. But a shellac disc is porous - not because of the shellac itself, but because of the fillers. As you know, if you subject a 78 to moisture (even high humidity), you will develop a grainy surface. That is due to the swelling of fibrous (porous) material imbedded in the surface of the shellac as it soaks up the moisture. Exposure to ultrasonic waves in a bath would seem to rapidly accelerate this process, as the solution permeates every available fissure at a molecular level. It may not be evident if you play the disc immediately after the bath, but eventually this phenomenon would manifest itself.


Of course, a laminated disc would be even more susceptible to damage - anywhere there is an opening, fluid will creep in. A crack or split would not need to be visible for this to occur, and the outer edge of the record would most assuredly be affected.

Comments and corrections welcome. (Indeed, I hope I'm wrong, as I have a large ultrasonic bath that could clean numerous discs at a time. The rotisserie feature would be easily constructed. I sometimes remove label stickers with spit, but this is the first time I've heard of using a spit to clean several discs at a time!)

Kurt Nauck

c/o Nauck's Vintage Records
22004 Sherrod Ln.
Spring, TX  77389

Website: www.78rpm.com
E-Mail: nauck@xxxxxxxxx

Phone: (281) 288-7826
Fax: (425) 930-6862


[Subject index] [Index for current month] [Table of Contents]