If this disk is somewhat akin to the later EvaTone Soundsheet, I've had very good luck playing those by placing them on top of a non-valued LP record. Another trick I've had success with is taping down the squared corners with regular old Scotch tape, so the disk lays flatter. This is not necessary all the time. I have dozens of EvaTone Soundsheets and have been able to transfer all of them with usually very good results.

-- Tom Fine

----- Original Message ----- From: "Wasserman, Robert A - WHS" <Robert.Wasserman@xxxxxxxxxxxxxxxxxxxx>
To: <ARSCLIST@xxxxxxxxxxxxxxxx>
Sent: Tuesday, July 17, 2007 4:15 PM
Subject: Re: [ARSCLIST] Playing a "flexi disc"



A suggestion, most modern turntables are not flat enough for these discs, place a piece of board or cardboard similar in size and shape of the disc with a hole in it to create a flat surface. You might need a small piece of tape on the back (if one sided) or near the edge if cardboard surface is too slippery.

Robert Wasserman
Robert.Wasserman@xxxxxxxxxxxxxxxxxxxx
Sound Archives Proj. Asst./Lead Tech.
Wisconsin Historical Society
608-264-6473




Dear Barbara Need,


If the disc is translucent green vinyl, it may be a Soundscriber
disc. These were 33.3 rpm microgroove, so you should try to play it
as if it were an LP. Pray that it hasn't warped; if it has, you may
need to send it to someone with excellent equipment and much experience.

Sincerely, Richard

At 02:59 PM 7/17/2007, you wrote:
I have been asked to get a digital transfer from what I believe to
be a "Flexi disc" (thin green plastic /vinyl disc with a square
hole). The only complication is that, as far as I can tell, these
were LPs and, therefore, no earlier than 1948. The date on the disc,
however, is '43. We have an osmium stylus (which we use for
78s)  and a diamond stylus (which we use for LPs). What stylus
should I use for playback? (And if you have recommendations for
adding to my stylus supply, I would welcome that as well, though I
may not be able to do anything about it just yet.)

Barbara