Peter @ specsbros wrote:
> To drive the mold into dormancy, it is necessary to remove
> moisture from the mold, itself, and the tape. This can take
> up to 8 - 10 days of holding the tape in a controlled
> environment of around 30% RH. It can be done somewhat faster
> at lower RH and can take quite a lot more time if the RH is higher.
> (Note: baking is not recommended as, while it can sometimes
> work, it can also cause problems with moldy tape- depending
> on the type and amount of mold, baking can harden the
> mold-related residues and "bake" wraps together).
So, it sounds like you are recommending a low-humidity exposure at normal
temperature for several days followed by cleaning.
What if the tape also has a bad case of SSS? It seems as though you would be
stopped. You can't spool it to clean it because it has SSS and you can't
bake it to spool it because it has mold.
What do you recommend?