[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
[ARSCLIST] Paper on Mold Removal from Cellulose Acetate Audiotape
The following [long - 63 p.] paper may be of interest:
"Research on Methods to Remove Mold from Cellulose Acetate Audiotape"
by Jim Thurn (Kilgarlin Center, U. Texas Austin)
http://www.ischool.utexas.edu/~anagpic/2006pdf/2006ANAGPIC_Thurn.pdf
- Walter Cybulski
Preservation & Collection Mgmt.
National Library of Medicine
Note: The paper is posted on the Association of North American Graduate
Programs in the Conservation of Cultural Property (ANAGPIC) website:
http://www.ischool.utexas.edu/~anagpic/index.htm