[Table of Contents]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

Re: [ARSCLIST] DAT Archival Housing



At 02:43 PM 2007-02-17, Farris Wahbeh wrote:
List,
Any suggestions on how to archival-ly house DAT tapes would be most helpful.
Are the plastic cases that they come with archival-ly sound? What are some boxes that can be used
to house the tapes? Has anyone come across a box that fits both DAT and CD's together?
I can't seem to find any in the Gaylord catalog.

That's because they and the machines they play on are not archival. The only archival way of storing a DAT tape IMHO is to transfer it to a digital repository or a gold phthalocyanine dye CD-R, with the former method preferred. DATs are living on borrowed time. THey are far more fragile than analog open reel and fewer machines were produced (I think) and few if any machines are being made now...just like open reel in a much shorter timeframe.


Cheers,

Richard


Richard L. Hess email: richard@xxxxxxxxxxxxxxx
Aurora, Ontario, Canada (905) 713 6733 1-877-TAPE-FIX
Detailed contact information: http://www.richardhess.com/tape/contact.htm
Quality tape transfers -- even from hard-to-play tapes.



[Subject index] [Index for current month] [Table of Contents]