Re: [ARSCLIST] Ampex 456



At 06:51 AM 6/16/2006, Lars Gaustad wrote:
Hi,
I have got a 2" Apmex 456 that is really sticky.
I has been stored at 8 C 35% RH for 8 years,
which makes me believe that the stickyness is not related to hydrolysis
(SS),
as such storage should rejuvenate the tape just as well as baking will.

Any suggestions?

Baking should still rejuvenate it if past history is any guide. I'm looking for a good explanation of precisely why baking works, but I've been told by people who understand these things that the generally accepted explanation is not the whole story.


There does appear to be mounting evidence that there is interaction between the back coat and the oxide binder system. Again, no answers at this time.

I'm not being mysterious, I'm slowly studying this.

Thanks for a really useful data point.

Many of the people working on this are not on this list and I'm taking the liberty of passing on your observations to them.

Cheers,

Richard


lars gaustad
preservation adviser
national library of norway
www.nb.no

Richard L. Hess email: richard@xxxxxxxxxxxxxxx
Aurora, Ontario, Canada (905) 713 6733 1-877-TAPE-FIX
Detailed contact information: http://www.richardhess.com/tape/contact.htm
Quality tape transfers -- even from hard-to-play tapes.



[Subject index] [Index for current month] [Table of Contents]