Hi Marcos

My understanding is that MAM are what Mitsui Gold's were.  Same formula,
different manufacturer and new name (I think!).

Cheers

Marie

Marie O'Connell
Sound Archivist/Audio Engineer/Sound Consultant
The Center For Oral History & Cultural Heritage
The University Of Southern Mississippi
118 College Drive #5175
Hattiesburg, MS, 39401-406
Ph: 601-266-6514
Fax: 601-266-6217
 
-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx] On Behalf Of Marcos Sueiro
Sent: Tuesday, April 25, 2006 7:13 AM
To: ARSCLIST@xxxxxxxxxxxx
Subject: [ARSCLIST] Medical grade CD-Rs

Greetings,

I just became aware of what they call "medical grade" CD-Rs. I was trying 
to figure out what is the difference, if any, between these and gold CD-Rs, 
and I was wondering if anyone has experience with these media.

<http://www.mam-a.com/products/medical/index.html>