[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] Recording Disc Preservation/Off-gassing?
I suspect the sleeves are the bad actor, and I doubt that it is off-gassing
but rather the plasticizer in the sleeves themselves. I have seen similar
sleeves used to store 35mm slides that were supposed to be "archival" cause
similar goo and patterning where they came into contact with the film
(unfortunately).
I would suggest that you try a different solvent that might provide better
results then water. You might try some surfactants although I doubt that the
results will be very good. The tackiness will probably still remain but I
would then move on to slightly more aggressive solvents. You might find that
ISO would do the job. I do not claim to know anything about the
sensitivities of the disks you have - so that is of course the first
priority - but with other media I have sometimes had some success with
common ISO - lab grade with a lower percentage of water and Texwipes. I have
used ISO Swabs sold in the local pharmacy on occasion - they work well but
may lint in your application. If that did not work - I might take a sample
of the sleeve and the gook to a friendly university chemist to figure out
precisely what you have - and then find a solvent that is unfriendly to the
gook but friendly to the disk chemistry. If the gentle solvents don't work -
there is no shortage of very aggressive solvents that will certainly remove
the goo - lighter fluid for example works on many different plasticizers and
there are commercial products like "goop off" but they may also destroy the
recordings - so be very careful. Parenthetically - I have seen markings like
the ones you mention that while visible do not interfere with the playback
since the contamination only occurred on the top surface of the recording
and not inside the groove.
jim
*