In a message dated 2/2/2004 1:04:07 AM Eastern Standard Time, ArcLists@xxxxxxxxxxxxxxx writes:
I think there are many people on the list who can gently play tapes. I can *******************
I have found reels of the cheap green boxed "Shamrock" brown oxide mylar tape that shed oxide in sheets leaving clear base. That is probably why it ended up in those boxes.
The oxide sheets just fell off as the tape was unwound; no bond to the base at all. It would be very hard to salvage.