[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [ARSCLIST] stability of shellac disks
Since everyone is on the discussion of glass. Has anyone ever researched or worked on reassembling broken glass records? I was once having a discussion with a friend that blows glass and I was wondering, if a cracked glass record ccould be put back together again with "hot" freshly blown glass. Any ideas?
Lance Watsky
Preservation & Media Specialist
The Georgia Archives
5800 Jonesboro Road
Morrow, GA 30260
678-364-3764 (phone)
678-364-3860 (fax)
lwatsky@xxxxxxxxxxxxxxx
www.GeorgiaArchives.org
-----Original Message-----
From: Association for Recorded Sound Discussion List
[mailto:ARSCLIST@xxxxxxx]On Behalf Of Aaron Luis Levinson
Sent: Friday, January 30, 2004 10:14 AM
To: ARSCLIST@xxxxxxxxxxxx
Subject: Re: [ARSCLIST] stability of shellac disks
This thickening is due to the way pane glass was manufactured
in the 19th century and earlier not due to its deformation as a
super-cooled liquid.
aa
On Friday, January 30, 2004, at 09:55 AM, Bewley, Nigel wrote:
> Okay...how do we account for window glass that has become thicker at
> the
> bottom of the pane than at the top? Apparently glass 'flows' over
> time -
> years not weeks - and window panes change shape!
>
> Nigel
> British Library
>
> -----Original Message-----
> From: Don Cox [mailto:doncox@xxxxxxxxxxxxxx]
> Sent: 30 January 2004 15:00
> To: ARSCLIST@xxxxxxxxxxxx
> Subject: Re: [ARSCLIST] stability of shellac disks
>
> On 30/01/04, Art Shifrin wrote:
>> "I have shellac records over a century old which exhibit no
>> deterioration other than wear!
>> Steven C. Barr"
>>
>> How do you know that the disks have not in some way changed or
>> deteriorated?
>>
>> Yes, they're playable but even glass changes shape over time.
>
> I saw an exhibition of Roman glass a few years ago. Those bottles etc
> didn't show any signs of having changed shape over 2000 years.
>
> Regards
> --
> Don Cox
> doncox@xxxxxxxxxxxxxx
>
>
> ***********************************************************************
> ***
>
> Experience the British Library online at www.bl.uk
>
> Adopt a Book this season ! Help the British Library conserve the
> world's
> knowledge. www.bl.uk/adoptabook
>
> ***********************************************************************
> **
>
> The information contained in this e-mail is confidential and may be
> legally
> privileged. It is intended for the addressee(s) only. If you are not
> the
> intended recipient, please delete this e-mail and notify the
> postmaster@xxxxx : The contents of this e-mail must not be disclosed or
> copied without the sender's consent.
>
> The statements and opinions expressed in this message are those of the
> author and do not necessarily reflect those of the British Library. The
> British Library does not take any responsibility for the views of the
> author.
>
> ***********************************************************************
> **
>