Re: [ARSCLIST] External A/D converter with AES/EBU output



From: Patent Tactics, George Brock-Nannestad

Graham Newton wrote:

> andy kolovos wrote:
>
> > I'm looking for recommendations for an external 24/96 A/D converter with
> > AES/EBU output.
>
> An excellent pro-quality stand alone A-D/D-A converter is the "ADA" made by
> CEDAR of England, primarily to work with their flagship Cambridge restoration
> system, but very useful on it's own, at less than US $1,000.
>

----- actually it is a RedBox made by Sonifex, only colored black when sold
by CEDAR. Check for yourselves at their website (not to hand). I am a
satisfied user of that.

Kind regards,

George