It would be useful to know what cassette brands
and product numbers have developed sticky-shed. If there is a date of
recording as well, that could contribute to identifying those at risk. Of
course, this does not "date" that tape but gives some idea of when it was in
use.
****
Have no numbers,
but from my experience:
Intermagnetics brand from the mid-80s
**All** types of Memorex
Anonymous, studio made cassettes - really any era
These are the major squealers in my collection.
David N. Lewis