Course:Lab Methods III
Date Offered:Fall Semester, 1997
Location:Peterborough, Ont. Canada
Instructor:Lana Dryden
Institution:Sir Sandford Fleming College

Syllabus

Description
This course provides an introduction to the types of materials, techniques, applications, and methods available for the treatment, stabilization, and optimum care for textile, paper, parchment and vellum artifacts. The identification, treatment, and stabilization of decorative surfaces, including colourants, pigments and applied finishes, are examined.

Aim & Learning Outcomes
Aim:
To provide the student with a basic understanding of conservation methods and conservation materials relating specifically to textiles, paper, parchment and vellum.
Learning Outcomes:
Students will have demonstrated the ability to:
know cleaning procedures for textiles, paper, parchment and vellum using a variety of techniques, (eg. dry cleaning, aqueous solutions, solvents, etc.)
know repair, consolidation and gap filling, supporting and stabilizing techniques for textiles, paper, parchment and vellum while maintaining the integrity of the original.
know techniques for colour tinting, colour matching and painting of replacement fills and surfaces for textiles, paper, parchment and vellum.
know mounting and display techniques for textiles, paper, parchment and vellum.

Course Format
This course is one of four courses listed in the "super module" of Conservation and Material Science III. Courses in this frame work are linked tightly together, and are interdependent to each other, and are foundation courses for the programme.
This course will consist of 2 hours of scheduled lectures per week. Lecture time may be subject to occasional adjustment in order to fit in with field trips, community based projects, group projects or guest lectures and/or workshops. Students are asked to remain flexible during the delivery of this course.
Additional time outside of scheduled class will be required for independent study and artifact treatment.

Course Content

DateLecture
Week 1
September 2 - 5
Labour Day
Week 2
September 8 - 12
Textile Conservation
- examination and recording
Week 3
September 15 - 19
Textile Conservation, Fiber Sample and Burn Test Workshop
Week 4
September 22 - 26
Textile Conservation Cleaning- mechanical
- spot removal
- aqueous
- drying
Week 5
September 29 - October 3
Mounting Workshop
Week 6
October 6 - 10
Textile Conservation
- supports, repairs
- storage, handling, display
Week 7
October 14- 17
Thanksgiving
Week 8
October 20 - 24
Independent Study Week
Week 9
October 27 - 31
Condition Report and Treatment Proposal Test, textiles
Week 10
November 3 - 7
Conservation of Paper
- examination
- cleaning
Week 11
November 10 - 14
Conservation of Paper
- repair
- consolidation
Week 12
November 17 - 21
Technology of Structure Workshop
Week 13
November 24 - 28
Conservation of Paper, support and mounting
- storage
- handling
- display
Week 14
December 1 - 5
Conservation of Parchment and Vellum
Lab Supply/Equipment List due
Week 15
December 8 - 12
Conservation of Other Paper Materials (papyrus, etc.)
Treatment Card Collection due

Evaluation
following criteria will be used to evaluate students' mastery of the theoretical and practical aspects of artifact examination, condition reporting, treatment proposal and treatment of objects made of ceramics, glass, stone and metals.

ITEMVALUE IN PERCENTAGEDUE DATE
Case Studies of Published Artifact Treatments of Paper Artifacts20%October 17, 1997
Condition Report and Treatment Proposal Test30%October 27, 1997
Lab Supply/Equipment List20%December 1, 1997
Treatment Card Collection30%December 8, 1997

Course Policies
Students must complete all course assignments in order to receive a passing grade.
Late assignments will be penalized 10% per day. Exceptions may be granted due to circumstances beyond the student's control, provided that the student contacts the instructor promptly upon return to the College to discuss alternate arrangements.

Academic Policies
1. Presentation
Written assignments must be:
typed or word-processed
double spaced
proofed for spelling and grammatical errors
enclosed with a single cover sheet which includes student name, title of the assignment and date of submission
stapled in the top left hand corner (unbound)
include a bibliography (where appropriate)
use a recognized method of citation (eg. MLA or Chicago)
2. Re-writes
Faculty may request a re-write of a submission if the criteria for assessment have not been met.
Late penalties will apply if the assignment is not re-submitted the following day.
3. Penalties for Late Submissions
Completion of Term Work
All assignments must be completed in order for students to achieve a passing grade.
Late Assignments
Late assignments receive the following penalty:
Marks will be deducted at the rate of 10% per day for three days after which assignments are marked at zero.
Faculty are not obliged to provide feedback on assignments marked at zero.
Oral Presentations
Oral presentations and/or practical test or projects for evaluation must be delivered on the day scheduled. A "no show" will be graded at zero, unless adequate explanation is provided.
4. Academic Integrity
Plagiarism is a serious breach of academic integrity and the college has a strict policy on this issue (see Academic Regulations).
It is a student's responsibility to ensure that all written submissions include an appropriate method of in text citation as well as an accompanying bibliography.
Seminar and oral presentations should be supported by a bibliography and sources should be referred to during the presentation.
5. Make-up Tests
In valid circumstances (ill-health, personal crisis), a student may
Students must contact the instructor within seven days of the original test in order to request a make-up.
6. Extensions & GDFS
An extension may be granted to an individual student based on need and circumstance. Medical grounds should be substantiated.
The revised due date will be recorded and signed by both parties.
The entire class may be given an extension, at the discretion of faculty.
Incomplete a Grade Deferred marks at the end of the semester must be negotiated between student and faculty (see Academic Regulations). Note: these are a privilege to be granted under special circumstances, not used in order to compensate for poor planning.
7. Site Work
Students must agree to work within the parameters of the guidelines established for site work. Failure to comply, may result in the termination of project and suspension of the privilege of access.

Readings:
No books required for this course.

Prerequities: NA

[Search all CoOL documents]