Picture Spot3

Spot3
Download TIFF file (~2 MB)
Silver gelatin glass negative (Courtesy of S. Dobrusskin). Repetitive three-spot pattern of silver mirroring. On the upper side: mirroring with shape similar to the round opening of the storage envelope.