Picture Non-processed1

Nonprocessed1
Download TIFF file (~2 MB)
Silver gelatin glass negatives. Cueni study collection (~1910). Non-processed and never used glass plates found still wrapped in the original black paper. The two plates have been packed with emulsion sides facing. Note that the silver mirroring edge pattern is exactly the same on the two plates.