TESTING CORROSION INHIBITORS FOR THE CONSERVATION OF ARCHAEOLOGICAL COPPER AND COPPER ALLOYS
Robert B. Faltermeier, Ph.D., B.Sc., Cert., Dipl.Cons. r.faltermeier@ucl.ac.uk
Figure 1: Coupon covered with nantokite and cuprite-50 microns
Copyright © Robert B. Faltermeier, 1997. All rights reserved.