AATCC. 2001a. Colorfastness to light, Option E, 16-1998. Research Triangle Park, N. C.: American Association of Textile Chemists and Colorists.

AATCC. 2001b. Ageing of sulfur-dyed textiles: Accelerated, alternate oven test, 26-1999. Research Triangle Park, N. C.: American Association of Textile Chemists and Colorists.

AATCC. 2001c. Instrumental color measurement: Evaluation procedure 6. Research Triangle Park, N. C.: American Association of Textile Chemists and Colorists.

ASTM. 2001a. Standard test methods of identification of textile fibers, D276-00a. West Conshohocken, Pa.: American Society for Testing Materials.

ASTM. 2001b. Standard test method of breaking force and elongation of textile fabrics, D5035-95. West Conshohocken, Pa.: American Society for Testing Materials.

ASTM. 2001c. Standard test method of stiffness of fabrics, Option A, D1388-96. West Conshohocken, Pa.: American Society for Testing Materials.

Blum, D.1982. An evaluation of some uses of synthetic resins in textile conservation. Proceedings of the Symposium on Resins in Conservation, Edinburgh, U. K., May 21-22. Scottish Society for Conservation and Restoration, 81–88.

Down, J. L.1984. Adhesive testing at the Canadian Conservation Institute, past and future. In Preprints of the Contributions to the Paris Congress. London: International Institute for Conservation of Historic and Artistic Works. 18–21.

Down, J. L.1986. The yellowing of epoxy resin adhesives: Report on high-intensity light aging. Studies in Conservation31:159–70.

Down, J. L., M. A.MacDonald, J.Tetreault, and R. S.Williams. 1996. Adhesive testing at the Canadian Conservation Institute: An evaluation of selected poly (vinyl acetate) and acrylic adhesives. Studies in Conservation41: 19–44.

Feller, R. L.1994. Accelerated aging: Photochemical and thermal aspects. Ann Arbor, Mich.: Edwards Brothers.

Feller, R. L., and D. B.Encke. 1982. Stages of deterioration: The examples of rubber cement and transparent mending tape. In Science and technology in the service of conservation: Preprints of the contributions to the Washington Congress,ed. N. S.Brommelle and G.Thompson. London: International Institute for Conservation of Historic and Artistic Works. 19–23.

Finch, K.1980. Changing attitudes—New developments—Full circle. In Conservation and restoration of textiles, ed.F.Pertegato. Milan: Centro Italiano per lo Studio della Storia del Tessuto. 82–86.

Himmelstein, P., and B.Appelbaum. 1977. The use of sprayed polyvinyl acetate resin mixtures in the mounting of textiles. Journal of the American Institute for Conservation17:37–44.

Horie, C. V.1987. Materials for conservation: Organic consolidants, adhesives and coatings. London: Butterworths.

Keyserlingk, M.1990. The use of adhesives in textile conservation. In ICOM Committee for Conservation Preprints. 9th Triennial Meeting, Dresden. Los Angeles: ICOM. 307–12.

Kronthal, L., J.Levinson, C.Dignard, E.Chao, and J.Down. 2003. Beva 371 and its use as an adhesive for skin and leather repairs: Background and a review of treatments. Journal of the American Institute for Conservation42:341–62.

Lombardi, R., and J.Gasper. 2001. Acrylic polymers. In Coatings and technology handbook, ed. D.Satas and A.Tracton. New York: Marcel Dekker. 391–402.

Masschelein-Kleiner, L., and F.Bergiers. 1984. Influence of adhesives on the conservation of textiles. In Preprints of the Contributions to the Paris Congress, ed. N.S.Brommelle, E. M.Pye, P.Smith, and G.Thompson. London: International Institute for Conservation of Historic and Artistic Works. 70–73.

Repp, J., and F.Yogerst. 2001. Fusible batting. U. S. Patent 6, 838, 398. Assigned to June Tailor Inc., Richfield, WI. Also available at www.uspto.gov/main/patents.htm.

Scott, B.2002. Personal communication. Therm O Web Inc., Wheeling, Ill.

Smith, J. A., ed.1983. Adhesives and coatings. Science for Conservators, Book 3. London: Crafts Council.

Stitch Witchery. 1969. Thermally activatable adhesive in net form. Trademark Serial Number 72319981. Assigned to Stitch Witchery, Stone Mountain, Ga. Also available at www.uspto.gov/trademarks.htm (accessed July 2002).

Timar-Balazsy, A., and D.Eastop. 1998. Chemical principles of textile conservation. London: Butterworths.

Wonder-Under. 1987. Fusible adhesive material for bonding fabrics. U. S. Trademark Serial Number 73670113. Assigned to Wonder-Under, Durham, N. C. Also available at www.uspto.gov/trademarks.htm (accessed June 2003).



SOURCES OF MATERIALS

505 Spray and Fix

JT Trading 3 Simm Lane Newtown, Conn. 06470 (203) 270-7744 fax: (203) 270-8746 www.sprayandfix.com

Sulky KK2000

Sulky of America 3113 Broadpoint Dr. Punta Gorda, Fla. 33983 (800) 874-4115 fax: (941) 743-4634 www.sulky.com

Sullivans Quilt-Basting Spray

Sullivans USA 4341 Middaugh Ave. Downers Grove, Ill. 60515 (800) 862-8586 www.sullivans.net/usa/default.htm

HeatnBond

Therm O Web 770 Glenn Ave. Wheeling, Ill. 60090 (800) 323-0799 (847) 520-5200 fax: (847) 520-0025 www.thermoweb.com

Stitch Witchery

HTC-Handler Textile Corp. 1717 Lilton Dr. Stone Mountain, Ga. 30083 (770) 938-7014 Fax: (770) 938-7018 htcann@aol.comwww.htc-handler.com

Wonder-Under

Pellon Consumer Products Division Freudenberg Nonwovens 3440 Industrial Dr. Durham, N.C. 27704 (800) 223-5275 fax: (908) 387-0152 www.pellonideas.com

Hobbs Heirloom 80% Cotton/20% Polyester Blend Fusible Batting, Hobbs Heirloom Bleached 100% Cotton Batting

Hobbs Bonded Fiber 200 South Commerce Dr. Waco, Tex. (254) 741-0040 (800) 433-3357 www.hobbsbondedfibers.com

June Tailor Low Loft Fusible Batting

June Tailor P.O. Box 208 2861 Highway 175 Richfield, Wisc. 53076 (800) 844-5400 (262) 644-5288 fax: (800) 246-1573, (262) 644-5061 www.junetailor.com/fusablebatting.htm

Mountain Mist White Gold 100% Cotton Fusible Batting, Mountain Mist Nonfusible 100% Polyester Batting

Stearns Technical Textiles Company 100 Williams St. Cincinnati, Ohio 45215 (513) 948-5275 (800) 345-7150 fax: (513) 948-5281 www.stearnstextiles.com/mountainmist/welcome.htm

Cotton Muslin

Testfabrics, Inc. P.O. Box 26 West Pittston, Pa. 18643 (570) 603-0432 fax: (570) 603-0433 www.testfabrics.com


AUTHOR INFORMATION

JANET EVENSON holds an MS in textile science from the University of Georgia and a PhD from the University of Nebraska–Lincoln with a specialization in textiles and a minor in museum studies. She is an assistant professor at Western Illinois University, where she teaches textile science courses. Address: 142 Knoblauch Hall, 1 University Circle, Macomb, Ill. 61455; j-evenson@wiu.edu

PATRICIA COX CREWS is Willa Cather Professor of Textiles, Department of Textiles, Clothing, and Design, and director of the International Quilt Study Center at the University of Nebraska–Lincoln (UNL). She has more than 20 years of research experience pertaining to the performance properties of textile materials. She teaches care and conservation of textile collections and textile history at UNL. Address: 204 HE Building, University of Nebraska–Lincoln, Lincoln, Neb. 68583-0802; pcrews@unl.edu


Copyright � 2005 American Institution for Conservation of Historic & Artistic Works