VERTICAL GRADIENTS OF POLLUTANT CONCENTRATIONS AND DEPOSITION FLUXES ON A TALL LIMESTONE BUILDING

VICKEN ETYMEZIAN, CLIFF I. DAVIDSON, SUSAN FINGER, MARY F. STRIEGEL, NOEMI BARABAS, & JUDITH C. CHOW




REFERENCES

Amoroso, G. G., and V.Fassina. 1983. Stone decay and conservation: Atmospheric pollution, cleaning, consolidation and protection, Materials Science monographs11. New York: Elsevier.

Appel, B. R., Y.Tokiwa, and M.Haik. 1981. Sampling of nitrates in ambient air. Atmospheric Environment15:283–89.

Bock, E., and W.Sand. 1993. A review: The microbiology of masonry deterioration. Journal of Applied Bacteriology74:503–14.

Braun, R. C., and M. J. G.Wilson. 1970. The removal of atmospheric sulphur by building stones. Atmospheric Environment4:371–78.

Cadle, S. H., and P. A.Mulawa. 1987. The retention of SO2 by nylon filters. Atmospheric Environment21:599–603.

Chan, W. H., D. B.Orr, and D. H. S.Chung. 1986. An evaluation of artifact SO42− formation on nylon filters under field conditions. Atmospheric Environment20:2397–2401.

Chow, J. C., J. G.Watson, L. C.Pritchet, W. R.Pierson, C. A.Frazier, and R. G.Purcell. 1993. The DRI thermal/optical reflectance carbon analysis system: Description, evaluation, and applications in U.S. air quality studies. Atmospheric Environment27a:1185–201.

Dabberdt, W. F., and W. G.Hoydysh. 1991. Street canyon dispersion: Sensitivity to block shape and entrainment. Atmospheric Environment25a:1143–53.

Davidson, C. I.1979. Air pollution in Pittsburgh: A historical perspective. Journal of the Air Pollution Control Association29:1035–41.

Davidson, C. I., S. E.Lindberg, J. A.Schmidt, L. G.Cartwright, and L. R.Landis. 1985. Dry deposition of sulfate onto surrogate surfaces. Journal of Geophysical Research90:2123–30.

Del Monte, M., C.Sabbioni, and O.Vittori. 1981. Airborne carbon particles and marble deterioration. Atmospheric Environment15:645–52.

DePaul, F. T., and C. M.Sheih. 1985. Measurements of wind velocities in a street canyon. Atmospheric Environment20:455–59.

Etyemezian, V., C. I.Davidson, and S.Finger. 1995. Influence of atmospheric pollutants on soiling of a limestone building surface. Progress report for the National Park Service, Pittsburgh. September. Carnegie Mellon University, Pittsburgh, Pa.

Etyemezian, V., C. I.Davidson, M. J.Zufall, W.Dai, S.Finger, and M.Striegel. 1998a. Impingement of rain drops on a tall building. Typescript. Carnegie Mellon University, Pittsburgh, Pa.

Etyemezian, V., N. R.Strader, C. I.Davidson, W.Dai, S.Finger, and M.Striegel. 1998b. Deposition of particles and surface soiling at a tall limestone building. Typescript. Carnegie Mellon University, Pittsburgh, Pa.

Fenter, F. F., C.Francois, and M. J.Rossi. 1995. Experimental evidence for the efficient “dry deposition” of nitric acid on calcite. Atmospheric Environment29:3365–72.

Freemantle, M.1996. Historic monuments pose challenge to conservation scientists. Chemical and Engineering News74:20–23.

Gould, T. R., C. I.Davidson, S.Finger, M. J.Small, and M. R.Lutz. 1993. Influence of atmospheric pollutant concentrations and deposition rates on soiling of a limestone building surface. Progress report for the National Park Service, Pittsburgh. May. Carnegie Mellon University, Pittsburgh, Pa.

Haneef, S. J., J. B.Johnson, C.Dickinson, G. E.Thompson, and G. C.Wood. 1992. Effect of dry deposition of NOx and SO2 gaseous pollutants on the degradation of calcareous building stones. Atmospheric Environment26a:2963–74.

Hering, S. V., D. R.Lawson, I.Allegrini, A.Febo, C.Perrino, M.Possanzini, J. E.SicklesII, K. G.Anlauf, A.Wiebe, B. R.Appel, W.John, J.Ondo, S.Wall, R. S.Braman, R.Sutton, G. R.Cass, P. A.Solomon, D. J.Eatough, E. C.Ellis, D.Grosjean, B. B.Hicks, J. D.Womack, J.Horrocks, K. T.Knapp, T. G.Ellestad, R. J.Paur, W. J.Mitchell, M.Pleasant, E.Peake, A.MacLean, W. R.Pierson, W.Brachaczek, H. I.Schiff, G. I.Mackay, C. W.Spicer, D. H.Stedman, A. M.Winer, H. W.Biermann, and E. C.Tuazon. 1988. The nitric acid shootout: Field comparison of measurement methods. Atmospheric Environment22:1519–39.

Hoydysh, W. G., and W. F.Dabberdt. 1994. Concentration fields at urban intersections: Fluid modeling studies. Atmospheric Environment28:1849–60.

Huber, A. H., S. PalArya, S. A.Rajala, and J. W.Borek. 1991. Preliminary studies of video images of smoke dispersion in the near wake of a model building. Atmospheric Environment25a:1199–1209.

Hutchinson, A. J., J. B.Johnson, G. E.Thompson, G. C.Wood, P. W.Sage, and M. J.Cooke. 1992. The role of fly-ash particulate material and oxide catalysts in stone degradation. Atmospheric Environment26a:2795–2803.

Hutchinson, A. J., J. B.Johnson, G. E.Thompson, G. C.Wood, P. W.Sage, and M. J.Cooke. 1993. Stone degradation due to wet deposition of pollutants. Corrosion Science34:1881–98.

Johansson, L. G., O.Lindqvist, and R. E.Mangio. 1988. Corrosion of calcareous stones in humid air containing SO2 and NO2. Durability of Building Materials5:439–49.

Judeikis, H. S., T. B.Stewart, and A. G.Wren. 1978. Laboratory studies of heterogeneous reactions of SO2∗. Atmospheric Environment12:1633–41.

Kirkitsos, P., and D.Sikiotis. 1995. Deterioration of Pentelic marble, Portland limestone and Baumberger sandstone in laboratory exposures to gaseous nitric acid. Atmospheric Environment29:77–86.

Lee, J. T., D. L.Call, R. E.LawsonJr., W. E.Clements, and D. E.Hoard. 1991. A video image analysis system for concentration measurements and flow visualization in building wakes. Atmospheric Environment25a:1211–25.

Lee, I. Y., and H. M.Park. 1994. Parametrization of the pollutant transport and dispersion in urban street canyons. Atmospheric Environment28:2343–49.

Livingston, R A.1992. Graphical methods for examining the effects of acid rain and sulfur dioxide on carbonate stones. Proceedings of the 7th International Congress on Deterioration and Conservation of Stone, Lisbon, Portugal. Lisbon: LNEC. 375–86.

Lutz, M. R., C. I.Davidson, S.Finger, T. R.Gould, M. J.Small, and V.Etyemezian. 1994. Influence of atmospheric pollutants on soiling of a limestone building surface, 1991–1994. Progress report for the National Park Service, Pittsburgh. September. Carnegie Mellon University, Pittsburgh, Pa.

McGee, E. S.1995. Sampling protocol used at the Cathedral of Learning in Pittsburgh, Pennsylvania. USGS Open-File Report 95–672, Reston, Va.

McGee, E. S.1997. Surficial alteration at the Cathedral of Learning in Pittsburgh, Pennsylvania. USGS Open-File Report 97–275, Reston, Va.

Meierding, T. C.1993. Marble tombstone weathering and air pollution in North America. Annals of the Association of American Geographers83 (4):568–88.

Mitchell, J. D., R.Gu, T. E.Ford, and N. S.Berke1996. Fungal degradation of concrete. Deutsche Gesellschaft f�r Chemisches Apparatewesen (DECHEMA) monographs133. Frankfurt, Germany: DECHEMA. 135–42.

Mossotti, V. G., and A. R.Eldeeb. 1994. Calcareous stone dissolution by acid rain. Typescript. Menlo Park, Calif.

Mulawa, P. A., and S. H.Cadle. 1985. A comparison of nitric acid and particulate nitrate measurements by the penetration and denuder difference methods. Atmospheric Environment19:1317–24.

Palmer, R. J., J.Siebert, and P.Hirsch1991. Biomass and organic acids in sandstone of a weathering building: Production by bacterial and fungal isolates. Microbial Ecology21:253–66.

Qin, Y., and L. Y.Chan. 1993. Traffic source emission and street level air pollution in urban areas of Guangzhou, South China (P.R.C.). Atmospheric Environment27b:275–82.

Qin, Y., and S. C.Kot. 1990. Validation of computer modeling of vehicular exhaust dispersion near a tower block. Building and Environment25:125–31.

Qin, Y., and S. C.Kot. 1993. Dispersion of vehicular emission in street canyons, Guangzhou City, South China (P.R.C.). Atmospheric Environment27b:283–91.

Sabbioni, C.1994. Effects of air pollution on historic buildings and monuments—Scientific basis for conservation: Physical, chemical, and biological weathering. European Cultural Heritage Newsletter on Research8(1):2–6.

Seinfeld, J. H., and S. N.Pandis. 1998. Atmospheric chemistry: Air pollution to global change. New York: John Wiley and Sons.

Sherwood, S. I., D. F.Gatz, R. P.HoskerJr., C. I.Davidson, D. A.Dolske, B. B.Hicks, D.Langmuir, R.Linzey, F. W.Lipfert, E. S.McGee, V. G.Mossotti, R. L.Schmiermund, and E. S.Spiker. 1990. Processes of deposition to structures. Report 20 in National Acid Precipitation Assessment Program, Acidic Deposition: State of Science and Technology, vol. 3. September.

Spedding, D. J.1969. Sulphur dioxide uptake by limestone. Atmospheric Environment3:683.

Spiker, E. C., R. P.HoskerJr., V. C.Weintraub, and S. I.Sherwood. 1995. Laboratory study of SO2 dry deposition on limestone and marble: Effects of humidity and surface variables. Water, air, and soil pollution proceedings of the 1995 5th international conference on acidic deposition: Science and policy, acid reign '95, G�teborg, Sweden. 2679–85.

Tayler, S., and E.May1991. The seasonality of heterotrophic bacteria on sandstones from ancient monuments. In Biodeterioration of cultural property, ed.R. J.Koestler. New York: Elsevier. 390–91.

Thompson, R. S.1993. Building amplification factors for sources near buildings: A wind tunnel study. Atmospheric Environment27a:2313–25.

Warscheid, T., M.Oelting, and W. E.Krumbein. 1991. Physico-chemical aspects of biodeterioration processes on rocks with special regard to organic pollutants. In Biodeterioration of cultural property, ed.R. J.Koestler. New York: Elsevier. 397–99.

Wilmzig, M., and E.Bock. 1995. Endangerment of mortars by nitrifiers, heterotrophic bacteria and fungi. In Biodeterioration and biodegradation 9, ed.A.Bousher et al. Rugby, UK: Institution of Chemical Engineers. 195–97.

Winkler, E. M.1996. Important agents of weathering for building and monumental stone. Engineering Geology1:381–400.

Wolff, G. T.1984. On the nature of nitrate in coarse continental aerosols. Atmospheric Environment18:977–81.

Wu, Y. L., C. I.Davidson, D. A.Dolske, and S. I.Sherwood. 1992. Dry deposition of atmospheric contaminants: The relative importance of aerodynamic, boundary layer, and surface resistances. Aerosol Science and Technology16:65–81.

Young, P.1996a. Mouldering monuments. New Scientist152:37–38.

Young, P.1996b. Pollution-fueled “biodeterioration” threatens historic stone. Environmental Science and Technology30:206a–8a.

Zappia, G., C.Sabbioni, and G.Gobbi. 1993. Non-carbonate carbon content on black and white areas of damaged stone monuments. Atmospheric Environment27a:1117–21.



SOURCES OF MATERIALS

Polyethylene Bags

Clean Room Products Inc., 1800 Ocean Ave., Ronkonkoma, N.Y. 11779-6532

Polycarbonate Membrane Filters

Costar, One Alewife Center, Cambridge, Mass. 02140

Ion Chromotagraph

Dionex Corp., 228 Titan Way, Sunnyvale, Calif. 94088-3603

Methanol

Fisher Scientific, 711 Forbes Ave., Pittsburgh, Pa. 15219-4785

Teflon Zefluor and Nylasorb Filters

Gelman Sciences, 600 S. Wagner Rd., Ann Arbor, Mich. 48106

Metering Valve

Hoke, One Tenakill Park, Cresskill, N.J. 07626

Stainless Steel Filter Holders

Millipore Corp., 80 Ashby Rd., Bedford, Mass. 01730

Quartz Fiber Filters

Pallflex Corp., 125 Kennedy Dr., Putnam, Conn. 06260

Teflon Filter Packs

Savillex Corp., 6133 Baker Rd., Minnetonka, Minn.55345

Dry Test Meter

Singer Corp., Product division closed

Laser Particle Counters

TSI Inc., P.O. Box 64394, St. Paul, Minn. 55164

Potassium Carbonate Impregnated Cellulose Filter

Whatman, 9 Bridgewell Place, Clifton, N.J. 07014


AUTHOR INFORMATION

VICKEN ETYEMEZIAN is a doctoral student at Carnegie Mellon University (CMU). He received combined bachelor degrees in physics and engineering from Occidental College and the California Institute of Technology, respectively, and a master's of science in environmental engineering from the Johns Hopkins University. His research has focused on the effects of atmospheric pollutants on sensitive building materials, with an emphasis on dry deposition and surface rain washing. Some of his other interests include policies for sustainable environments in developing countries, urban and remote atmospheric chemistry, contaminant transport in groundwater, and innovative solutions for wastewater treatment. Address: Department of Civil and Environmental Engineering, Carnegie Mellon University, Pittsburgh, Pa. 15213.

CLIFF I. DAVIDSON is professor of civil and environmental engineering and engineering and public policy at Carnegie Mellon University (CMU). He is also director of the Environmental Institute at CMU. His main research interests involve atmospheric pollutants, focusing on the way particles and gases are transported through the atmosphere, the mechanisms by which particles and gases deposit from the atmosphere onto different types of surfaces, and historical trends in air pollution levels. His main educational activities include developing material that can be used broadly in basic science and engineering courses to increase student awareness of environmental issues. Address as for Etyemezian.

SUSAN FINGER is on the faculty of the Civil and Environmental Engineering Department at Carnegie Mellon University. She is also affiliated with the Engineering Design Research Center, the Robotics Institute, and the Department of Mechanical Engineering. She is a founder and co-editor-in-chief of the journal Research in Engineering Design. Her research interests include representation languages for designs, integration of design and manufacturing concerns, and computer-aided engineering. Address as for Etyemezian.

MARY F. STRIEGEL currently serves as the materials research program coordinator for the National Center for Preservation Technology and Training, where she is responsible for the supervision of in-house and external research on the effects of air pollution on cultural resources. Before going to NCPTT, she was a researcher with the Getty Conservation Institute. She holds bachelor degrees in fine arts and chemistry from the University of Louisville, a master's degree in analytical chemistry from Indiana University–Purdue University in Indianapolis, and a doctoral degree in inorganic chemistry from Washington University in St. Louis. Address: National Center for Preservation Technology and Training, NSU, Box 5682, Natchitoches, La. 71497.

NOEMI BARABAS received a bachelor's of science degree in chemical engineering and public policy with a minor in environmental engineering from Carnegie Mellon University. She is completing work on a master's degree (with subsequent Ph.D.) in environmental engineering in the Water Resources and Environmental Engineering Program at the University of Michigan. Her interests are water resource management and policy and its application in Eastern Europe. Address: Department of Civil and Environmental Engineering, University of Michigan, 116 EWRE Building, 1351 Beal Ave., Ann Arbor, Mich. 48109.

JUDITH C. CHOW, research professor in the Energy and Environmental Engineering Center (EEEC) at the Desert Research Institute (DRI), University and Community College system of Nevada, has more than 19 years of experience in conducting air quality studies and performing statistical data analysis. She directs DRI's Environmental Analysis Facility, where she supervises filter processing and chemical operations. Dr. Chow has extensive experience in program planning; ambient and source sampling from urban and nonurban areas; gravimetric, x-ray fluorescence, atomic absorption spectrophotometric, ion chromatographic, automated colorimetric, and thermal/optical reflectance carbon analyses of filter samples, as well as interpretive statistical data analyses, principal component analyses, such as multivariate statistical analysis, and chemical mass balance receptor modeling. Address: Desert Research Institute, 5625 Fox Ave., P.O. Box 60220, Reno, Nev. 89506.


Copyright � 1998 American Institute for Conservation of Historic and Artistic Works