RESCUING WATER-DAMAGED TEXTILES DURING THE LOS ANGELES RIOTS

DUBRAVKA TURKOVIC-KISELJEV



1 INTRODUCTION

During the period of urban unrest in Los Angeles from April 29 to May 2, 1992, a portion of the costume and textile study collection belonging to the Los Angeles County Museum of Art (LACMA) was subjected to water damage. The damage occurred in an off-site storage area, access to which was not immediately available due to the concern for staff safety. This paper describes the course of action and the rescue effort.