JAIC 1990, Volume 29, Number 2, Article 8 (pp. 207 to 220)
JAIC online
Journal of the American Institute for Conservation
JAIC 1990, Volume 29, Number 2, Article 8 (pp. 207 to 220)

MEASURING THE RATE OF ATMOSPHERIC CORROSION IN MICROCLIMATES

HARALD BERNDT




REFERENCES

ASTM. 1981. Preparing, cleaning, and evaluating corrosion test specimens, G1-81; Conducting atmospheric corrosion tests on metals, G50-76. In Annual book of ASTM standards: Wear and erosion, vol. 03.02, Metal corrosion. Philadelphia: American Society for Testing and Materials.

Arni, P. G., G. C.Cochrane, and J. D.Gray. 1965a. The emission of corrosive vapours by wood, I: Survey of the acid-release properties of certain freshly felled hardwoods and softwoods. Journal of Applied Chemistry15: 305–13.

Arni, P. G., G. C.Cochrane, and J. D.Gray. 1965b. The emission of corrosive vapours by wood, II. The analysis of the vapours emitted by certain freshly felled hardwoods and softwoods by gas chromatography and spectrophotometry. Journal of Applied Chemistry15: 463–68.

Bennet, C. A., and N. L.Franklin. 1954. Statistical analysis in chemistry and the chemical industry. New York: John Wiley and Sons.

Berndt, H.1987. Assessing the detrimental effects of wood and wood products on the environment inside display cases. AIC preprints, 15th Annual Meeting, American Institute for Conservation, Vancouver, British Columbia. 22–33.

Blackshaw, S. M.1982. The testing of display material. Museum Ethnographers Group occasional paper no. 1. 40–45.

Blackshaw, S. M., and V. D.Daniels. 1978. Selecting safe materials for use in the display and storage of antiquities. ICOM Committee for Conservation preprints, 5th Triennial Meeting, Zagreb, 23/2/1–23/2/9.

Budde, W. L., and J. W.Eichelberger. 1979. Organics analysis using gas chromatography/mass spectrometry: A techniques and procedures manual. Ann Arbor, Mich: Ann Arbor Science Publishers.

Carpenter, J. M., and P. B.Hatchfield. 1987. Formaldehyde: How great is the danger to museum collections?Cambridge, Mass.: Center for Conservation and Technical Studies, Harvard University Art Museums.

Clarke, S. G., and E. E.Longhurst. 1961. The corrosion of metals by acid vapours from wood. Journal of Applied Chemistry11: 435–43.

Connolly, M. D.1987. Creating microenvironments in airtight cabinets—a warning: Statement of preliminary findings. AIC Newsletter12(4):5–6.

Devorkin, H., R. L.Chass, and A. P.Fudurich. 1972. Air pollution source testing manual. Los Angeles County, Calif: Air Pollution Control District.

Donovan, P. D., and J.Stringer. 1969. Corrosion of metals by acid vapors. Extended abstracts, 4th International Congress on Metallic Corrosion, Amsterdam, The Netherlands. 133–36.

Donovan, P. D., and J.Stringer. 1971. Corrosion of metals and their protection in atmospheres containing organic acid vapours. British Corrosion Journal6: 132–38.

Donovan, P. D., and T. M.Moynehan. 1965. The corrosion of metals by vapours from air-drying paints. Corrosion Science5: 803–14.

FitzHugh, E. W., and R. J.Gettens. 1971. Calclacite and other efflorescent salts on objects stored in wooden museum cases. In Science and archaeology, ed.R. H.Brill. Cambridge, Mass: MIT Press. 91–102.

GCI. Newsletter.1987. Microenvironmental research. Getty Conservation Institute Newsletter2(3):7.

GCI. Newsletter. 1988. Environmental research in conservation. Getty Conservation Institute Newsletter3(2): 1–2.

Hatchfield, P. B., and J. M.Carpenter. 1986. The problem of formaldehyde in museum collections. International Journal of Museum Management and Curatorship5: 183–88.

Leveque, M. A.1986. The problem of formaldehyde: A case study. AIC preprints, 14th Annual Meeting, American Institute for Conservation, Washington, D.C.56–65.

Miles, C. E.1986. Wood coatings for display and storage cases. Studies in Conservation31: 114–24.

Oddy, W. A.1973. An unsuspected danger in display. Museums Journal73: 27–28.

Oddy, W. A.1975. The corrosion of metals on display. In Conservation in archaeology and the arts, ed.N. S.Brommelle and P.Smith. London: International Institute for Conservation of Historic and Artistic Works. 235–37.

Packman, D. F.1957. Corrosion of cadmium plated steel by plywood and wood assemblies made with synthetic resin glues. Forest Products Research Laboratory report 77646.

Packman, D. F.1960. The acidity of wood. Holzforschung14: 178–83.

Padfield, T., D.Erhard, and W.Hopwood. 1982. Trouble in store. In Science and technology in the service of conservation, ed.N. S.Brommelle and G.Thomson. London: International Institute for Conservation of Historic and Artistic Works. 24–27.

Schniewind, A. P.1989. Strength. In Concise encyclopedia of wood and wood-based materials, ed.A. P.Schniewind. Cambridge, Mass: MIT Press. 245–50.

Scully, J. C.1975. The fundamentals of corrosion. Oxford: Pergamon Press.

Thomson, G.1978. The museum environment. London: Butterworths.

Weast, R. C., ed.1979. CRC handbook of chemistry and physics, sec. B. Boca Raton, Fla.: CRC Press.

Wilcox, W. W.1989. Decay during use. In Concise encyclopedia of wood and wood-based materials, ed.A. P.Schniewind. Cambridge, Mass: MIT Press. 71–75.

Youden, W. J.1951. Statistical methods for chemists. New York: John Wiley and Sons.


AUTHOR INFORMATION

HARALD BERNDT has been assistant specialist at the University of California Forest Products Laboratory, Wood Artifacts Conservation and Timber Mechanics Group, since 1985. He is the 1989–90 vice president/program chair of the Bay Area Art Conservation Guild. He holds an M.S. degree in wood science and technology from the University of California, Berkeley, and the degree of Diplom-Holzwirt from the University of Hamburg, Germany. He has published articles in the ACS Symposium Series, Journal of Wood Conservation, and AIC preprints. Address: University of California at Berkeley, Forest Products Laboratory, 1301 South 46th St., Richmond, Calif. 94804.