CRITERIA FOR TREATMENT: REVERSIBILITY
Barbara Appelbaum
7 AESTHETIC ADDITIONS
In this area, the highest requirements for reversibility should be applied. Compensation and protective coatings should be easily removable without removing or weakening structural parts of a treatment.
|