CONSERVATION OF LEATHER AND TEXTILES FROM THE DEFENCE

Kenneth Morris, & Betty L. Seifert



4 A CONSERVATION TREATMENT FOR TEXTILES FROM THE DEFENCE

LINEN, HEMP, AND SILK have been the fibre-contents of the textiles recovered from the site of the DEFENCE. The treatment presented below was used in the conservation of these textiles to impart flexibility and stability.