VOL. 13 (2012), No. 3

METHODS OF AQUEOUS TREATMENTS
The Last Resort for Badly Damaged Iron Gall Ink Manuscripts


WÄSSRIGE BEHANDLUNG VON TINTENTRASS
Letzter Ausweg für schwer geschädigte Eisengallusmanuskripte


Author/Autorin: Véronique Rouchon, Marthe Desroches, Valeria Duplat, Marine Letouzey, Julie Stordiau Pallot
Abstract: The calcium phytate treatment has given rise to intensive research. Despite its efficiency largely having being demonstrated, this treatment is not used on badly damaged manuscripts mainly because water is used as a solvent. Indeed, exposing badly damaged paper to aqueous solutions is paired with a substantial risk of causing additional splits and losses, which has so far hindered the use of calcium phytate on the most vulnerable manuscripts. This work investigates ways of manipulating badly damaged manuscripts during aqueous treatments. It was first tried out on test samples then originals. The results showed that mechanical risk is greatly minimized when the treatment is performed by flotation and with specific handling and drying precautions.
Zusammenfassung: Die Calciumphytatbehandlung ist Gegenstand intensiver Forschungsarbeit. Obwohl ihre Wirksamkeit hinlänglich erwiesen ist, wird sie bei stark geschädigten Handschriften nicht angewandt, da Wasser als Lösungsmittel zum Einsatz kommt. Tatsächlich kann eine wässrige Behandlung zu weiteren Rissen und Substanzverlust im behandelten Papier führen. Daher wurde bislang bei derart gefährdeten Handschriften meist auf eine Phytatbehandlung verzichtet. Die vorliegende Arbeit untersucht verschiedene Methoden, stark geschädigte Manuskripte wässrig zu behandeln. Die Tests wurden zunächst an Probepapieren dann an Originalen durchgeführt. Die Ergebnisse zeigten, daß sich das Risiko mechanischer Schäden deutlich verringert, wenn man das Papier schwimmend wässert und besondere Vorkehrungen bei seiner Handhabung und Trocknung trifft.
Keywords: Methodology (Using Test Samples to Evaluate the Mechanical Risk - From Test Samples to Original Manuscripts) - Results (Evaluation of the Most Hazardous Sample Treatment Step - Optimizing the Sample Removal Method from the Solutions - Optimising the Drying Process - Investigating the Lining Process - Use on Highly Damaged Originals) - Conclusion - Acknowledgements - Endnotes - References - Suppliers - Authors


YAK-HIDES, CASES, BOXES, ENCLOSURES AND OTHER WRAPPINGS OF ORIENTAL OBJECTS AT THE ROYAL LIBRARY, COPENHAGEN

YAK-HÄUTE, KÄSTCHEN, SCHACHTELN, UMSCHLÄGE UND ANDERE VERPACKUNGEN ORIENTALISCHER GEGENSTÄNDE DER KÖNIGLICHEN BIBLIOTHEK, KOPENHAGEN

Authors/Autoren: Bent Lerbaek Pedersen
Abstract: Over the years the Oriental Department of the Royal Library has received Oriental objects sent from the Far East in many types of wrappings. This article deals in part with the original packing of shipments and in part, with the protection of the objects on the shelves of the library. Everything is based on examples from the Oriental Collection, i.e. manuscripts, block prints and other printed materials from Asia.
Zusammenfassung: Im Laufe der Jahre erhielt die Abteilung für Orientalische Kunst zahlreiche Objekte aus dem Fernen Osten, die sehr unterschiedlich verpackt waren. Dieser Artikel beschäftigt sich sowohl mit den originalen zum Versand verwendeten Verpackungen als auch mit den Aufbewahrungsformen in den Regalen der Bibliothek. Die behandelten Fallstudien basieren alle auf Beispielen aus der Orientalischen Sammlung, darunter Handschriften, Holzschnitte und andere Drucke aus Asien.
Keywords: Shipments - Objects with Culturally Determined Protective Materials (North Africa and Western Asia - South and Southeast Asia - Tibet and Mongolia - China, Japan and Korea - Indonesia) - Boxing and Packing Materials in the Library - Boxing Material Today - Endnote - Author


EDITORIAL

'If Author Ye Will Be, The Guidelines Ye Must Read' (Véronique Rouchon)


IADA NEWS

IADA Board Meeting - The New Website - IADA Network at LinkedIn - IADA Symposium 2013 - IADA News in Brief (Roland Damm) - New Members

IN PRACTICE

The Conservation of Two Oversized Film Posters: Case Study of Image Reintegration Solutions for Paper-Based Artefacts (Magdalena Grenda)

Do Safes Protext Modern Laser-Printed Documents? (Jonas Palm)

Mounting Papyri: Example of Mounting a Papyrus Collection of the Islamic Art Department in the Louvre Museum (Aurelia Streri)

INSTRUCTABLES

An Aqueous Treatment for Highly Damaged Manuscripts: Minimising the Risk of Mechanical Damage (Marthe Desroches, Valéria Duplat, Véronique Rouchon)

> If you have a clever, pragmatic idea that you want to share with our readers, please contact Bas van Velzen


MATERIALS & EQUIPMENT

Bench-Top Ionizing Air Blower (Leila Sauvage)

> If you want to share information on new 'Materials & Equipment'; in the field of book and paper conservation, please contact Claire Phan Tan Luu or Dionysia Christoforou

DEGREE WORKS

L'Institut National du Patrimoine:
- Magali Bonnet: Conservation Treatment of a 19th Century Spanish Doll's House - Development of a Dry Consolidation Technique for Ornamental Paper on Wood

The Royal Danish Academy of Fine Arts Kopenhagen:
- Kathleen Mühlen: A Systematic Description at Microscopic Level of the Dimensions of Parchment Fibers Before and During Shrinkage

> If you want to provide abstracts of master-thesis degree works in the field of book, paper and photograph conservation, please contact Istvan Kecskemeti


ONLINE SUPPLEMENT


LITERATURE

Recent Publications | Neue Veröffentlichungen

Book Reviews | Rezensionen

Bookbinding and Conservation (Gerd Brinkhus)
Etherington, Don: Bookbinding and Conservation. A sixty-year Odyssey of Art and Craft. Foreword by Bernard Middleton. New Castle: Oak Knoll Press 2010. ISBN 978-1-58456-277-1. 156 S., 53 Farbtafeln. GBP 49,95. > PDF

Nineteenth-Century American Paper and Mediums (Hildegard Homburger)
Baker, Cathleen A: From the Hand to the Machine. Nineteenth-Century American Paper and Mediums: Technologies, Materials, and Conservation. Ann Arbor, MI: The Legacy Press, 2010. 432 pp, numerous ill. ISBN 978-0-9797974-2-2. USD 65,00. > PDF

Leonardo in neuem Lichte (Georg Dietz)
Ambers, Janet, et al. (Eds.): Italian Renaissance Drawings: Technical Examination and Analysis. London: Archetype Publications, 2010. 183 pp, numerous illustrations. ISBN 978-1904982586. EUR 49,80. > PDF

Suggested Readings | Zeitschriftenauswertung


News: Berühmtes Kartenwerk entdeckt - Variante von Amerikas "Geburtsurkunde" in der UB | Archives & Libraries > PDF

TRAINING

Training Events | Fortbildungskalender


EXHIBITIONS

Exhibition Calendar | Ausstellungskalender

ADVERTISEMENTS

Römerturm Feinstpapier GmbH & Co KG, DE-50226 Frechen

IADA - International Association of Book and Paper Conservators, DE-37073 Göttingen

Fototext Verlag Wolfgang Jaworek, DE-70180 Stuttgart

Geräte, Material und Werkzeuge für Papierrestauratoren Gabi Kleindorfer, DE-84186 Vilsheim

Hans Schröder GmbH, DE-76689 Karlsdorf-Neuthard

Werkstatt für Papier, Dipl. Ing. Gangolf Ulbricht, DE-10997 Berlin, gangolf.ulbricht@p-soft.de

Karthäuser-Breuer GmbH, DE-50777 Köln

Föll-Vertriebs-GmbH, DE-50777 Köln

Hamburger Buntpapier Susanne Krause, DE-22559 Hamburg

Franz Hoffmann, Bucheinbandleder und Pergamente, Inh. Thomas Schmidt, DE-70197 Stuttgart

Schempp Bestandserhaltung GmbH, DE-70806 Kornwestheim

Klug Conservation, Walter Klug GmbH & Co. KG, DE-87509 Immenstadt

Anton Glaser Feinpapiergroßhandlung, DE-70174 Stuttgart

Tru Vue, Inc. - Optium Acrylic Products, US-McCook, IL



[HOME] [IADA] [PUBLIKATIONEN] [KONTAKT] [IMPRESSUM]
© IADA - Online-Publisher: Wolfgang Seidel
This page last changed: September 1, 2012

[Search all CoOL documents]  [CoOL] [Feedback]