It's fun to find outdoor sculpture! This sculpture depicts two children playing and
dancing. They are dressed for a warm summer day. What articles of clothing will these
children need in winter? A sweater? Boots? What else? Bronze sculptures like this one also
need protection from the outdoor elements. A coating of wax can be used to help protect
the bronze from air pollution, weather, birds and graffiti.